Tribological problems in shaft hoist ropes wear process

Czasopismo: Industrial Lubrication and Tribology   Tom: 67, Zeszyt: 1, Strony: 157-164
ISSN:  0036-8792
Wydawca:  EMERALD GROUP PUBLISHING LIMITED, HOWARD HOUSE, WAGON LANE, BINGLEY BD16 1WA, W YORKSHIRE, ENGLAND
Opublikowano: 2015
 
  Autorzy / Redaktorzy / Twórcy
Imię i nazwisko Wydział Katedra Procent
udziału
Liczba
punktów
Michał Styp-Rekowski20.00  
Eugeniusz Mańka20.00  
Maciej Matuszewski20.00  
Monika Madej orcid logoWMiBMKatedra Mechaniki**2010.00  
Dariusz Ozimina orcid logoWMiBMKatedra Mechaniki**2010.00  

Grupa MNiSW:  Publikacja w czasopismach wymienionych w wykazie ministra MNiSzW (część A)
Punkty MNiSW: 20
Klasyfikacja Web of Science: Article


DOI LogoDOI     Web of Science Logo Web of Science    
Keywords:

Lifting rope  Magnetic test  Mining hoist  Steel construction  Tribological wear 



Abstract:

Purpose - The purpose of this paper was to create conditions for the correct decision concerning an exchange of the used rope for a new one. A cognitive goal was to indicate the causes of its wear and determining its mechanism reliability and durability.

Design/methodology/approach - The magnetic, organoleptic and strength standard tests of lifting triangle-strand ropes of a mining hoist were carried out. This way the current state of the tested rope was defined.

Findings - On the basis of an analysis of the results of the performed tests: magnetic, organoleptic and fatigue tests, it can be said that the magnetic one is accurate enough only to indicate the place of the rope's biggest weakening, though the degree of weakening is not defined precisely - with significant excess. The accurate rope's destruction degree is indicated by the strength tests.

Practical implications - The results of described investigations can improve safety of the mining rope mechanisms operation, even for an increased resource.

Originality/value - The elementary wear processes, which are the basic reason for the destruction of the rope, are indicated. Rope destruction is caused mainly by tribological factors: abrasion, corrosion and fatigue wear. Magnetic tests are accurate enough only to indicate the place of the rope's biggest weakening (qualitative index). Most precisely, the rope's destruction degree (quantitative index) can be found by the strength tests.